Suzhou Crystal Base New Materials Co.,Ltd
Welcome Visitors to Booth No. 1146 GlassBuild America Oct.19-21,2016 Las Vegas Nevada,USA
Place of Origin: | China |
Brand Name: | Crystal Base |
Certification: | CE/CSI/BS/ASTM |
Model Number: | TSG |
Minimum Order Quantity: | 100sqm |
---|---|
Price: | negotiation |
Packaging Details: | Packed in Strong Plywood Crates or Cases with PE,paper or Saftpad interlayer |
Delivery Time: | 15 days after order confirmed |
Payment Terms: | T/T ,L/C,DP or western Union |
Supply Ability: | 3,000 Sqm per Day |
Product Name: | Tempered Safety Glass | Application: | Glass Panel, Glass Cabinets, |
---|---|---|---|
Size Of Panel: | Various | Colours: | Clear, Ultra Clear, Various Green, Blue, Gray, Brown. |
Standard: | CE/CSI/BS/ASTM | Type: | Flat Or Curved Sheet Glass |
Thickness: | 3-19mm | Transmittance: | More Than 88% |
High Light: | frameless glass pool fence,glass swimming pool fence |
15mm Curve Toughened Glass Pool Fencing , Safety Decorative Pool Fencing
Specification:
Product |
Toughened Glass |
Other Names |
Toughed Glass/Safety glass/ Tempered glass with heat soak test |
Specification |
Flat Tempered Glass Max size 18000mm*3660mm Min size 300mm*100mm Curved Tempered Glass Min curved radius 450mm Arc of length: Max 3600mm Min300mm Height: Max 18000mm Min300mm |
Authentication |
CCC (China Compulsory Certification) ;BS EN14179-1:2005/BS6206:1981; CE EN12150-1:2000: GB/T19001-200idtISO9001:2000 |
Construction Use |
Glass Door, Curtain Wall Partition, Elevator, Showcase |
Household Use |
Sanitary glass, Cabinet, Furniture glass. |
Color |
Clear, Ultra Clear, Various Green, Blue, Gray, Brown. |
Thickness:3-19mm
Description
Toughened glass is used when thermal resistant,strength and safety are the primary considerations.
Toughened glass is most commonly found in the side and rear window of automobiles.
Toughened glass is also widely used in building,for frameless glass doors,slider doors or any application
where human contact and safety are considerations.Cell phones sometimes have tempered glass in their construction,because of its durability and scratch resistant quality.
Tempered glass is also used for cooking and baking utensils.
Toughened glass production process
1. Cutting : cutting the annealing glass to the actual needs of shape.
2. Glass edging: Edging machine to mill the four edges to prevent frund when steeling,while
maintaining the beautiful appearance.
3. Drilling hole:If need to drilling hole using drilling machine.
4. Washing dry:cleaning the glass with washing maching.
5. Tempered glass:Tempered glass is produced by heating annealed glass in a furnace to 700°,
then the glass is rapidly cooled with jets of cold air to 40°,through the procedures, the original